Gresnigt, M M; Özcan, M; Kalk, W; Galhano, G (2011). Effect of static and cyclic loading on ceramic laminate veneers adhered to teeth with and without aged composite restorations. Journal of Adhesive Dentistry, 13(6):569-577.

[img]Published Version
PDF - Registered users only
283kB

View at publisher

Abstract

PURPOSE:

Existing composite restorations on teeth are often remade prior to the cementation of fixed dental prostheses. The aim of this study was to evaluate the effect of static and cyclic loading on ceramic laminate veneers adhered to aged resin composite restorations.
MATERIALS AND METHODS:

Eighty sound maxillary incisors were collected and randomly divided into four groups: group 1: control group, no restorations; group 2: two Class III restorations; group 3: two Class IV restorations; group 4: complete composite substrate. Standard composite restorations were made using a microhybrid resin composite (Anterior Shine). Restored teeth were subjected to thermocycling (6000 cycles). Window preparations were made on the labial surface of the teeth for ceramic laminate fabrication (Empress II). Teeth were conditioned using an etch-and-rinse system. Existing composite restorations representing the aged composites were silica coated (CoJet) and silanized (ESPE-Sil). Ceramic laminates were cemented using a bis-GMA-based cement (Variolink Veneer). The specimens were randomly divided into two groups and were subjected to either static (groups 1a, 2a, 3a, 4a) or cyclic loading (groups 1b, 2b, 3b, 4b). Failure type and location after loading were classified. Data were analyzed using one-way ANOVA and Tukey's test.
RESULTS:

Significantly higher fracture strength was obtained in group 4 (330 ± 81 N) compared to the controls in group 1 (179 ± 120 N) (one-way ANOVA, p < 0.05). Group 1b survived a lower mean number of cyclic loads (672,820 cycles) than teeth of groups 2b to 4b (846x103 to 873x103 cycles). Failure type evaluation after the fracture test showed predominantly adhesive failures between dentin and cement, but after cyclic loading, more cohesive fractures in the ceramic were seen.
CONCLUSION:

Ceramic laminate veneers bonded to conditioned aged composite restorations provided favorable results. Surface conditioning of existing restorations may eliminate the necessity of removing aged composite restorations.

Citations

3 citations in Web of Science®
1 citation in Scopus®
Google Scholar™

Altmetrics

Downloads

2 downloads since deposited on 22 Feb 2012
0 downloads since 12 months

Detailed statistics

Additional indexing

Item Type:Journal Article, refereed, original work
Communities & Collections:04 Faculty of Medicine > Center for Dental Medicine > Clinic for Fixed and Removable Prosthodontics
DDC:610 Medicine & health
Language:English
Date:2011
Deposited On:22 Feb 2012 09:48
Last Modified:03 Dec 2013 14:24
Publisher:Quintessence Publishing
ISSN:1461-5185
Publisher DOI:10.3290/j.jad.a21742
PubMed ID:21734979

Users (please log in): suggest update or correction for this item

Repository Staff Only: item control page